10. Fooladfar H., Hasnemi B., and Younesi M. The effect of the surface treating and high-
temperature aging on the strength and SCC susceptibility of 7075 aluminum alloy //
J. Mater. Engng. Perform. – 2010. – 19. – P. 852–859.
11. Comparison of SCC thresholds and environmentally assisted cracking in 7050-T7451
aluminum plate / E. M. Arnold, J. J. Schubbe, P. J. Moran, and R. A. Bayles // Ibid. – 2012.
– 21. – P. 2480–2486.
12. U. S. Patent 3856584. Reducing the susceptibility of alloys, particularly aluminium alloys, to
stress corrosion cracking / B. M. Cina. – 1974.
13. Reda Y., Abdel-Karim R., and Elmahallawi I. Improvements in mechanical and stress
corrosion cracking properties in Al-alloy 7075 via retrogression and re-aging // Mater. Sci.
Eng. A. – 2008. – 485. – P. 468–475.
14. Influence of repetitious-RRA treatment on the strength and SCC resistance of Al–Zn–Mg–Cu
alloy / G. Peng, K. Chen, S. Chen, and H. Fang // Mater. Sci. Engng. A. – 2011. – 528.
– P. 4014–4018.
15. Su R. M., Qu Y. D., and Li R. D. Effect of aging treatments on the mechanical and corrosive
behaviors of spray-formed 7075 alloy // J. Mater. Eng. Perform. – 2014. – 23. – P. 3842–3848.
16. Effect of aging treatments on microstructure and exfoliation corrosion behavior of spray
forming 7075 alloy / R. M. Su, Y. D. Qu, R. D. Li et al. // Adv. Mater. Res. – 2013. – 774.
– P. 872–875.
17. Ohnishi T., Ibaraki Y., and Ito T. Improvement of fracture toughness in 7475 aluminum
alloy by the RRA (retrogression and re-aging) process // Mater. Trans. JIM. – 1989. – 30.
– P. 601–607.
18. U. S. Patent 4713216 K. Aluminum alloys having high strength and resistance to stress and
corrosion / K. Higashi, T. Ohnishi, and I. Tsukuda. – 1987.
19. U. S. Patent 5108520J. Heat treatment of precipitation hardening alloy / J. Lin, and M. M. Ker-
sker. – 1992.
20. Triple over-aging treatment of 7150 aluminum alloy / X. L. Han, B. Q. Xiong, Y. A. Zhang
et al. // Chin. J. Nonferrous Met. – 2012. – 22. – P. 3006–3014 (in Chinese).
21. Thirty years of retrogression and re-aging (RRA) / X. J. Wu, M. D. Raizenne, R. T. Holt et
al. // Canadian Aeronautics and Space Journal. – 2001. – 47, № 3. – P. 131–138.
22. Effect of aging on corrosion resistance of 7050 aluminum alloy pre-stretching plate / F. X. Song,
X. M. Zhang, S. D. Liu et al. // Chin. J. Nonferrous Met. – 2013. – 23. – P. 645–651 (in Chinese).
23. Wang D., Ni D. R., and Ma Z. Y. Effect of pre-strain and two-step aging on microstructure
and stress corrosion cracking of 7050 alloy // Mater. Sci. Engng. A. – 2008. – 494. – P. 360–366.